Heatreater101 Posted July 31, 2022 Share Posted July 31, 2022 Distortion during normalizing of AISI316 a popular austenitic stainless steel used for good corrosion resistance. I am trying to normalize a sphere machined from a rod of 316. How do I control during distortion during the heat treatment. Quote Link to comment Share on other sites More sharing options...
Steve Sells Posted July 31, 2022 Share Posted July 31, 2022 Normalizing should not effect it , its the Austenite/Martensite transformation that will change it Quote Link to comment Share on other sites More sharing options...
ThomasPowers Posted July 31, 2022 Share Posted July 31, 2022 For any process evenness of heat helps a lot. Quote Link to comment Share on other sites More sharing options...
Irondragon Forge ClayWorks Posted August 1, 2022 Share Posted August 1, 2022 Welcome from the Ozark mountains. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.