September 17, 20169 yr hey guys so today I heat treated cpm s35vn for the first time...its in the cryo tank now so in the morning I will finish with temper. my question is 59-60 the right hardness point to shoot for? for any of you that use this steel what do you shoot for in the heat treat?
September 17, 20169 yr Author well being the first one I will keep it for my self for testing but it is a design I have done in 440c up for sale as a general purpose EDC knife. here is a pic of one that was done in 440c