  1. I've been making cheese knives out of stainless steel shorts, so unknown grade stainless.

    I recently saw a post on instagram where the guy was forging stainless jewellery and he said he was pickling and passivating the stainless in aluminium sulphate before polishing.

    Googling explained what the pickling and passivating process is but I couldn't see any references to aluminium sulphate being used.

    Also if the passivating process leaves a coating only microns thick wouldn't polishing wear that coating off?

     

    Does Anybody have any experience with these processes?

     

     

  2. I started building this gas forge in December 2015 and it got mostly done with the exception of the mortar and paint.  Now Feb 2017 it has got those two items completed and has been put to use.

    It even cooks lunch while cooling down. Started with corn finished with a few snags.

     

    IMG_9732.JPG

    IMG_9733.JPG

    IMG_9734.JPG

    IMG_9735.JPG

    IMG_1180.JPG

    IMG_4568.JPG

  3. Since we have a 3 week old baby and I'm not getting any sleep I'm staying out of the smithy until I'm not a complete zombie.   Hopefully I'll either get used to no sleep or things will improve soon as I need to get things done.  In the meantime I'm researching the New Kinyon Design power hammer which hopefully I can't maim myself doing in  my sleep deprived state.

    Where can I find the latest iteration of the plans and have there been any advancements recently?  Is there a PDF version?

    I did see a video of a twin rod head on YouTube as opposed to the specified square run in UHMW guides.

    i need to find out what equivalent parts are available over here and do a costing on it

    I noticed some double hit when you stop is this common to all, what causes it and how do you resolve this?

     

     

  4. I asked for a link so I can see what it looks like.  I'm in Australia. We do have some Harris gear here but it comes from the Europe plant not the USA Milwaukee? Plant.

    so the models etc will have diff designations etc. and I'd have to tell the store guy this is the one I want to order in as they only sell a few of many different brands.

  5. Spot heat, heat treat & cut. Are what I'm focussed on. 

    Brazing I haven't seen a need.....yet.

    As for welding, I have 2 stick and a MIG. So that isn't a nessecity unless it can do something the others can't and is easy to learn.

     

    I looked a some LPG (similar to propane) torches that I wondered if they would get hot enough, fast enough?  Anyone used ser a straight propane kit?  I have the small disposable Mapp/Butane and want something much, much more effective.

    I also saw the LPG/Oxy sets which are about 20% cheaper than the Acetlyne kit the same. I'm told they work just as well but cheaper to run, although they can't weld. I assume therefore they are not quite as hot?

×
×