I used to have problems when finishing detailed ironwork with the traditional wax/boiled linseed oil/mineral spirits mix.
When dry, I would sometimes have wax build up in the hard to reach places leaving a pale yellow deposit that I didn't care for.
I found the answer by blowing compressed air in those unreachable places while the mix is still in the liquid state.
This still leaves the area protected with a coat of treatment without having to reach in with a rag.(and you can control the air pressure, I don't go at it agressively just enough to get the extra wax out).
This saves me a lot of frustration and time.

Naz

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...