Okay k26 brick installed and in the process of refractory order. Next question. How deep does the tip of the flare need to penetrate the forge? Right now I have it set flush with the inside face of the liner...as mentioned before lots of trouble getting it to light. After it warms up for 5-10 minutes it’s easier to light. Thoughts?