Hi all, have been lurking for some time now, (as my name suggests).
Finally broke down and bought a single burner forge off Amazon.
It didn't come with rigidizer, so I Used fumed silica and water.
While I have read many of your post about buttering or spraying water before applying satanite. I don't know if i used enough water. Was I suppossed to use a lot of water, like I did rigidizer. Where it was soaked? or just a misting so the satanite would stick? When I was applying, the satanite seemed to come off the ceramic blanket. (i read some where if there is too much water in the blanket , the refractory will blow it self off the fiber)
While I intend to do a double coating of satanite and then finish off with itc 296a (on sale), I don't want to fire it up only to have a bunch fall off and don't want to waste more satanite if I should start over. Think I should fire it up with the coating I have now and see, then apply my second coating, or would that cure the coating and the satanite won't stick to the current one that is on there? Meassurement of satanite was 1lbs weighed, to 130 ml water.
Second question, will itc 296a stick to satanite?
kind regards Shadow. (And yes this is my gaming name)