  1. No I am not using a drossing flux. Would that help with the holes in the ingot?
  2. What do you mean by degassing? Sorry I am a bit new to this.
  3. I thank you both for your feedback! I will try to cast another ingot with this new info.
  4. Can someone tell me how I can stop this from happening when I cast my ingots? I made sure the iron mold was plenty hot and made sure to pore the molten copper evenly.
×
×