stefalive
-
Posts
2 -
Joined
-
Last visited
-
hi daniel, Im going to make my first knifes with stock removal I'm in mexico now for hollidays and the steel available here is 110WCrV5 in your recent post: http://www.iforgeiron.com/forum/f14/forging-vs-stock-removal-7748/index2.html you mention that: if choosen the right steel(for example:110WCrV5,80WCrV8 or115W8)and normalizing them for 2 or 3 times they get carbides under 2 micron and outperforming the most forged blades. could you tell me how this normalizing process (2 or 3 times) is done? sincerly, Stefan my email: stefalive@gmail.com