What is the best 'clay' to use when making a hamon? I am using a high temp. furnace cement putty, but it makes a lot of bubbles when it cures and gives my blades an inconsistent pattern. I follow the directions on the tub of clay to apply, but it still does some weird stuff (cooling in random places where the clay comes off making a spotty pattern that doesn't look very good). Anyone know of something better to use?