21 hours ago, teenylittlemetalguy said:

Also please don't use flux, it provides no significant cleaning action and is just one more thing to get in the way of two CLEAN surfaces coming together.

 

Uh, Tristan weren't you just recently expounding on using soldering flux making a  mokume billet? Should I find the post? I have a lot of jeweler friends who dissolve borax in water as a brush on penetrating flux for precious metals.

Borax isn't a cleaner it's a prophylactic oxygen barrier.

Frosty The Lucky.

Link to comment
Share on other sites

  • 2 weeks later...

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...