I need 27 j impact energy at -20C temp. for s235j2 (C:0.1- Si:0.04- Mn:0.45- P: 0.025, S: 0.02)

what heat treatment cycle is good for this steel?

Share this post


Link to post
Share on other sites

Why not ask the place where you got the steel or the supplier of that type steel?  If they are using or selling the stuff they should also have the HT information.

Share this post


Link to post
Share on other sites

The supplier should be able to supply you a chart/graff showing tempering lines incorporating izod, uts, hardness etc.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this