Jump to content
I Forge Iron

Reeltree

Members
  • Posts

    330
  • Joined

  • Last visited

Everything posted by Reeltree

  1. called a super quench,,,with chlorine with a little bit of kiddie urine
  2. Nice lil jig , gonna do one to use up a bunch of broken hay rake teeth into hooks,,,I scraped the driveway from all the heavy rain storms the past few day,, cut the grass then refaced some hammers
  3. Saw an old dusty gallon of raw linseed oil beside the boiled linseed gallons in the old country hardware store the next county over. On the front of the can states " to use with iron and metal coating and finishes", at a little over $30.00 for the gallon. I can't recall seeing any raw linseed for quit some time or is it just my narrow vision
  4. Put this one together this week, wheels were a couple bucks at auction
  5. Yep, I liked the concept also,,, made up a large and small one today,,cut the bolt head off ,, welded on a one inch shank
  6. First off I was not talking life threatening or loose of limb situations Secondly I would hope most would know when the need for professional help is required Thirdly slam it all you wish for I need not respond anymore
  7. I have gone thru my 57 years of life with what works for me,, when living at the beach getting sun burned and showering in warm water and increasing the temp lil hotter at a time worked for me, minimal peeling, the same when I burn my self,, now mind you im not talking deep fryer oil to the hospital type, the other day I grabbed a piece of metal that was hot, hot enough to make those instant white marks on the fingers, did the increase hot water trick,, no blisters no soreness,, ya'll may think it to be a myth or not ,but has been working for me for years and years,, I do suggest you use your better judgment and Not use scalding water nor any type of cleaning products,, if you prefer the cooling sensation effect go for it, deal with the sore blisters
  8. nope cold will impregnate the heat which causes the blisters and soreness,
  9. which at sometime you may eventually grab that hot piece of metal, don't fret,, just run warm water over the burn gradually increasing the temp hotter and hotter for as long as you can stand it, this will draw the heat out of the burn,,really it does work as it works also on sunburn, I grabbed a piece yesterday ran it under hot water for a spell ,, today no blisters no sorness
  10. put an adjustable cover plate over the squirrel cage opening, made all the difference in getting the fire to burn
  11. I use hi temp paint on the inside and clay,, outside I get cheap spray paint at the dollar store,,
  12. punched out this stand last week for the 275 pounder
  13. finally got around to putting wheels on one forge and refurbishing a smaller one had to go with a hair dryer , the lil blower was 25 mhp wouldn't even get the fire lit
  14. I have the blower parts ,,the box has rusted away
  15. foodlion carries a cheap pure clay kitty litter,,be sure to grind it up first
  16. hey come on over to Nelson county and look at a couple I have for sale
  17. Gonna start refurbishing an old forge that has been setting around,,, has a western chief blower attached,,,one lil crack on end to weld..anyone have an idea what make it might be
  18. thx,, I liked vaughnT's idea with sockets,, I tryed deepwell,, works great
  19. fixed up some needed tools today for My new anvil,,also a set of ajustable benders
  20. Just finished a 6 1/4 vise and stand today,,2ft round and 2 inch thick base with 6x6 upright beam,,,the lil 4 /14 is an old peter wright
  21. Reeltree

    Show me your vise

    Just finished a 6 1/4 vise and stand 2ft round and 2inch thick base with 6x6 upright beam,,the lil 4 /14 vise is an old peter wright
×
×
  • Create New...