Bruce after polishing on a natural chug nagura stone (about 2000- 2500 grit) I give 'em a quick dip in a white vinegar & lemon juice Mix that I heat to near boiling in the microwave. Then I neurtalize with baking soda and rinse with water a couple of times then just oil the blade.